MEMSnet Home: MEMS-Talk: Re: Young's modulus of SiO2 and silicon nitride
Re: Young's modulus of SiO2 and silicon nitride
1996-07-18
OleSøndergård Jensen
1996-07-18
[email protected]
Re: Young's modulus of SiO2 and silicon nitride
OleSøndergård Jensen
1996-07-18
I have one reference on Youngs modulus of silicon nitride:
Sensors and Actuators 20(1989) pp. 135-141. They have measured
Youngs modulus of nitrid to:

290 GPa for LPCVD nitride
210 GPa for Plasma-CVD nitride

Youngs modulus will be dependent on the deposition parameters as these
numbers show.

Best regards

Ole Sondergard
Danfoss A/S
DK-6430 Nordborg
Denmark


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Addison Engineering