MEMSnet Home: MEMS-Talk: selectivity between silicon nitride and silicon
selectivity between silicon nitride and silicon
2002-03-07
Peng Yao
2002-03-07
Michael Pedersen
2002-03-07
[email protected]
selectivity between silicon nitride and silicon
Peng Yao
2002-03-07
Hi,
I am going to etch silicon using silicon nitride as the mask. But I only
have CF4, SF6, O2 and He... I am not sure if those gases are enough for my
application or I need to order some new gases.
Thanks.

Peng Yao
DOEs lab
Electrical Engineering Dept.
Univeristy of delaware
Newark D.E 19716

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
University Wafer