The thin plastic wafers(thickness<200um) is needed!!
Michael D Martin
2002-03-12
You can get polyimide films from 175 microns to 12.5 from Dupont.

>>> [email protected] 03/11/02 01:08PM >>>
Hi, there,

Do you know which company sell some thin plastic
wafers(thickness<200um)?

Thank you so much!

ZHU, Xiaoshan
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk

Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
MEMStaff Inc.
Mentor Graphics Corporation