Decon-Dalo Resist Pen Supplier
Roger Brennan
2002-03-18
Hi Kirk,

I found a Dalo resist pen on

http://www.megauk.com/artwork_aids.php

I hope this is the one you want.

Roger Brennan

-----Original Message-----
From:   [email protected] [SMTP:[email protected]]
Sent:   Monday, March 18, 2002 3:52 PM
To:     [email protected]
Subject:        [mems-talk] Decon-Dalo Resist Pen Supplier

Where can I buy a Decon-Dalo brand resist pen?
This looks like an ink pen, but writes a resist material
that can be used in plasma etching and other applications.
It is handy for quick tests and for touching up a bad photoresist spin.
A U.S. supplier is preferred. And no, they don't have them at Radio Shack.

        --Kirt Williams Agilent Technologies
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
The Branford Group
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.