UV cured silicones
2002-03-26
allen kine
UV cured silicones
allen kine
2002-03-26
A 1997 article  J.C. Lotters described the application of a UV cured PDMS
for MEMS structures.
The shear modulus was approximately 250,000 Pascals.

The  article used  ABCR851 ((methacryloxypropyl)methylsiloxane) with
2,2-dimethoxy 2-phenylacetopheneone catalyst. ABCR851 is not currently
shown on the ABCR website.

Is there a commercial UV cured silicone which would have a similar shear
modulus.
Is there a correlation between the shear modulus and the shore durometer
measurement?

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
MEMStaff Inc.