Re: Al oxide removal

You could remove the oxide in a plasma cluster load lock system and transfer
your substrate to the next step, keeping your substrate under vacuum.

Gordon Whitlock
Business Manager
Trion Technology
480-968-8818 x-11
[email protected]

-----Original Message-----
From: [email protected] [mailto:[email protected]]On
Behalf Of [email protected]
Sent: Saturday, March 30, 2002 9:01 AM
To: [email protected]
Subject: mems-talk digest, Vol 1 #239 - 1 msg


Send mems-talk mailing list submissions to
        [email protected]

To subscribe or unsubscribe via the World Wide Web, visit
        http://mail.mems-exchange.org/mailman/listinfo/mems-talk
or, via email, send a message with subject or body 'help' to
        [email protected]

You can reach the person managing the list at
        [email protected]

When replying, please edit your Subject line so it is more specific
than "Re: Contents of mems-talk digest..."


Today's Topics:

   1. Al oxide removal ([email protected])

--__--__--

Message: 1
To: [email protected]
From: [email protected]
Date: Fri, 29 Mar 2002 12:07:31 -0500
Subject: [mems-talk] Al oxide removal
Reply-To: [email protected]

Dear MEMS coworkers,

We currently utilize foundry service to fabricate our MEMS platform, and we
functionalize the platform by coating a proprietary material. The existing
platform design calls for, fresh out of foundry, a SiO2 top layer with
contact openings to the underlying Al.

The issue we run into is that the exposed Al is easily oxidized and the
contact resistance varies from sample to sample. We have tried using
chemistry removing the aluminum oxide layer prior to functionalization. Yet
the oxidation happens so rapidly that a  thin insulating oxide is formed
between sample transfer (in air), so we alleviated but not eliminated the
reproducibility difficulty.

I appreciate any insights.

Regards,

Barry Chen


--__--__--

_______________________________________________
mems-talk mailing list
[email protected]
http://mail.mems-exchange.org/mailman/listinfo/mems-talk


End of mems-talk Digest

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
Addison Engineering
Process Variations in Microsystems Manufacturing