MEMSnet Home: MEMS-Talk: Searching for a thin conductive material
Searching for a thin conductive material
2002-04-08
Bo He
2002-04-09
Faid, Karim
2002-04-10
Chunjun Wang
Searching for a thin conductive material
Chunjun Wang
2002-04-10
You might want to try ACF(Anisotropic Conductive Film). Sony Chemical sells
this kind of film. But I am not sure you can make them less than 1 um thick.

Good luck!

-----Original Message-----
From: Bo He [mailto:[email protected]]
Sent: Monday, April 08, 2002 8:20 PM
To: [email protected]
Subject: [mems-talk] Searching for a thin conductive material

Hello everyone:

         I am looking for a CONDUCTIVE material which is FLEXIBLE (i.e.
polymer) and can be made very THIN (about 1um or less, possible?). Can
anyone who has experience on this give me suggestions? Any input is
highly appreciated.

Bo



------------------------------------------------------------------------

Send and receive Hotmail on your mobile device: Click Here
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Harrick Plasma, Inc.
MEMS Technology Review