I Need SOI
Rick Williston
2002-04-10
To All

Due to unanticipated difficulties in processing, we find ourselves in short
supply of 4" SOI wafers critical to our MEMS development activities.  This
is a long-shot, but does anyone have any surplus SOI wafers with 1-2 micron
embedded insulator with 50-100 microns of silicon on top of it?  If so, send
me availability, numbers,  pricing, resistivity and name of the
manufacturer.  You can reply directly to my e-mail at
[email protected]
If I could get some wafers to tide me through until our next delivery
(preferably this week) it would really save my bacon!

Thanks
Rick

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
MEMStaff Inc.