A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Spinning BCB on Nitride.
Spinning BCB on Nitride.
2002-04-29
Noah Clay
2002-04-30
Lester Lopez
2002-04-30
Noah Clay
2002-05-01
Bill Moffat
Spinning BCB on Nitride.
Bill Moffat
2002-05-01
Noah,
     No experience with BCB starbursts but lots of experience with resist
spinning star bursts give me a call 408 954 8353 and I will unload on you.  Be
warned I will also talk at length about our BCB baking oven  Bill Moffat

-----Original Message-----
From: Noah Clay [mailto:[email protected]]
Sent: Monday, April 29, 2002 4:27 PM
To: [email protected]
Cc: [email protected]
Subject: [mems-talk] Spinning BCB on Nitride.


I'm having difficulty spinning BCB on nitride.  There appears to be a
consistent starburst or comet pattern on the wafer despite following the
manufacturer's instructions for dispensing the adhesion promoter and BCB
itself.  I'm using an eppendorf and dispensing until the wafer is
covered in the slow spin stage at 100RPM (I've tried not coating the
wafer completely, but the problem seems exacerbated in those instances).
I'm also dispensing at a level very close to the wafer and very
well-centered.  I've read that the comet pattern usually arises from air
bubbles in the BCB, but I've taken pains to allow settling prior to
dispense.  HELP!

Noah Clay
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
MEMS Technology Review
Process Variations in Microsystems Manufacturing