cleanup after silicon drie
2002-05-09
Olgica Bakajin
2002-05-09
[email protected]
cleanup after silicon drie
Olgica Bakajin
2002-05-09
What do you use to remove the teflon-like polymer (one of the most inert
things there are!) that gets stuck on the wafer during some RIE processes
(like the passivation layer in DRIE)?
I have tried 3:1 sulphuric:peroxide and oxygen plasma but that still
doesn't seem to fully take care of it -- some polymer still stays stuck in
the deep narrow trenches.
I need something that would attack the flourocarbons but not damage the
silicon.
Any ideas would be appreciated.
--Olgica
Lawrence Livermore National Lab

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
MEMS Technology Review
Nano-Master, Inc.