2002-05-13
Though I don't have experience etching fused silica, perhaps the techniques I
have used to etch Pyrex would be applicable.

Since  photoresist doesn't adhere well to Pyrex, I use a chrome layer on the
Pyrex as an adhesion layer/etch mask.

If an isotropic profile is acceptable, buffered oxide etch (1.7 microns/hr for
Pyrex), or HF solution should work.  If an anisotropic profile is desired, a
fluorine based RIE process, such as SF6/O2 should suffice (5 microns/hr for
Pyrex).

Roger Shile

>>> [email protected] 05/10/02 12:07PM >>>
Hi all,

I was wondering if anyone could suggest the "best" way of creating a swimming
pool like structure about 20 microns deep in a piece of fused silica.
Basically, I need a trench with a known depth for fluid film thickness
calibrations.  Any ideas or preferred companies for this?

Thanks,
Edward
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.