A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Highest resistivity silicon?
Highest resistivity silicon?
2002-05-20
Fred Hussain
2002-05-20
Michael Pedersen
2002-05-20
David Nemeth
2002-05-20
Michael Barger
2002-05-20
Kenneth Smith
2002-05-22
mmf
2002-05-20
Kenneth Smith
2002-05-20
Michael D Martin
Highest resistivity silicon?
Michael Barger
2002-05-20
Fred,

I guess I need to weigh in here. The intrinsic resistivity of silicon is 240
kOhm-cm as indicated on the tydex web site. This is the theoretical limit.
It also mentions that 30 kOhm-cm is available. Generally, this is about the
best you are going to get. Anything that you do to this material will reduce
the resistivity, period. The degree to which you are careful will determine
how much the resistivity will be reduced. The highest resistivity material
that I have ever seen was 100 kOhm-cm, which was probably close to a world
record. I was able to get a 3-inch diameter boule of this material from
Westinghouse in the early 90's. Unfortunately, they did not and do not sell
silicon commercially and my contacts are no longer there.

Good luck,

Mike Barger
Klesis Corporation


-----Original Message-----
From: [email protected] [mailto:[email protected]]On
Behalf Of David Nemeth
Sent: Monday, May 20, 2002 11:44 AM
To: [email protected]
Subject: RE: [mems-talk] Highest resistivity silicon?


First, 250 K-Ohm cm seems like an unrealistically high value.  I've seen
silicon up to 12 KOhm-cm, and have used material up to 6KOhm-cm.  Looking at
the web site, they don't actually seem to produce this value - it might just
be the theoretical resistivity of pure silicon with no dopants that they are
quoting.

There are other suppliers of high-resistivity silicon, for example wacker
and topsil.

Next, I've heard (but can't say for sure) that if you grow a thermal oxide,
the resistivity will never be higher than a few thousand ohm-cm when your
done, no matter how good it was to start.  Any thermal treatment will
diffuse some impurities into the wafer, depending on the time and
temperature of the treatment.

If you need to end up with 2000 ohm-cm, your probably fine.  If you need to
end up with 6000 ohm-cm, you will need to be careful about your thermal
processing and may have problems.  If you need 250000 ohm-cm, your probably
out of luck.


David Nemeth
Senior Process Engineer
Sophia Wireless, Inc.
14225-C Sullyfield Circle
Chantilly, VA
Ph: (703) 961-9573 x206
Fax:(703) 961-9576

-----Original Message-----
From: [email protected] [mailto:[email protected]]On
Behalf Of Fred Hussain
Sent: Monday, May 20, 2002 6:47 AM
To: [email protected]
Subject: [mems-talk] Highest resistivity silicon?


Dear all,

I am looking for silicon substrates which can be machined using conventional
MEMS type processes, but at the same time are highly insulating. I've found
a web page with silicon of 250Kohm-cm resistivity -
http://www.tydex.ru/materials/materials2/Si.html.

Does anybody:
have any experience of working with such materials?
know of any issues, for example the stability of the resistivity with
temperature?
micromachined it without any major issues?
know of any suppliers?

Thanking you in advance.

Regards,

Fred.

--------------------------------------------
Dr Fred Hussain
The Technology Partnership plc
Melbourn Science Park
Cambridge Road
Melbourn
Royston
Hertfordshire
SG8 6EE

Tel: 01763 262626
Fax: 01763 261582
www.ttpgroup.com
---------------------------------------------
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
MEMS Technology Review