A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: HF and photoresist mask
HF and photoresist mask
2002-05-30
Jing Liu
2002-05-30
Mighty Platypus
2002-05-30
Bill Moffat
2002-05-30
Henry Yang
2002-05-30
[email protected]
2002-06-03
Soojin Oh
2002-05-31
Jing Liu
2002-05-31
Mighty Platypus
metal-glass bonding and debonding
2002-06-03
carlton watson
2002-05-31
Greg Miller
2002-05-31
Bill Moffat
2002-05-31
Bill Moffat
2002-05-31
Bill Moffat
2002-05-31
Jing Liu
2002-05-31
Roger Shile
HF and photoresist mask
Roger Shile
2002-05-31
My experience in etching SiO2 with unbuffered HF was pinholes in the SiO2
regions under photoresist (the HF seemed to go through the photoresist).

Photoresist does, however, provide an effective mask when etching with
Buffered Oxide Etch (HF + NH4F).

Roger Shile

>>> [email protected] 05/30/02 12:34PM >>>
To who may concern,

I want to mask HF etching with photoresist. Just now, somebody suggest me
that
for the same thickness of oxide I will etch. The photoresist could stand
buffered HF, but for concentrated HF, it will not. Is it exactly the case?
Could I be able to find some reference?

BTW, we have Shipley 1813, AZ 5214, Az 9245 in the lab. Does anyone have some
date of how fast they will etched in HF?

Thanks,

Jing
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

"This email and any attachments may contain information that is confidential
and proprietary information of Veeco Instruments Inc. and are intended only
for the use of the addressee. Unauthorized use, distribution or copying is
forbidden. If you have received this email in error, please notify the sender
immediately by return email and delete all copies of this message and any
attachments from your computer. Thank you."

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
The Branford Group
Addison Engineering
University Wafer