backside protection
2002-06-05
Roger Shile
2002-06-06
Mac McReynolds
2002-06-06
Scott Sullivan
backside protection
Scott Sullivan
2002-06-06
There are tapes made by Mitusi, Lintec, and Nitto that are chemical
resistant tapes.  These are mainly used as backgrind tapes.  Nitto, Lintec,
and Furukawa make UV releasing dicing tape.  If you cannot find their phone
numbers P-mail me and I will send them to you.

Scot




"Roger Shile"  on 06/05/2002 05:06:45 PM

Please respond to [email protected]

To:    [email protected]
cc:     (bcc: Scott Sullivan/Disco_Corp)
Subject:    [mems-talk] backside protection



I am looking for a tape to put on the backside of 100 mm Si wafers to
preserve
the oxide on the back, while etching the front in buffered oxide etch.

I have seen this done using dicing tape.  A coworker told me about
something
called "Yellow Tape" that came in circular pieces the same size as the
wafer,
apparently made for this purpose.  After use, the Yellow Tape was removed
with
acetone, which would be an advantage over peeling dicing tape from delicate
substrates.

Could someone refer me to a source for this Yellow Tape or suggest an
alternative?

Roger Shile

"This email and any attachments may contain information that is
confidential
and proprietary information of Veeco Instruments Inc. and are intended only
for the use of the addressee. Unauthorized use, distribution or copying is
forbidden. If you have received this email in error, please notify the
sender
immediately by return email and delete all copies of this message and any
attachments from your computer. Thank you."
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
MEMStaff Inc.