MEMSnet Home: MEMS-Talk: Silicon oxynitride optical properties
Silicon oxynitride optical properties
2002-06-28
kakasaheb chandrakant mohite
2002-06-28
MJ
Silicon oxynitride optical properties
MJ
2002-06-28
Dear K.C.Mohite

We have some results for SiOxNy deposited by PECVD and optomechanical
characteristics (residual stress versus refractive index).
  a.. S.S. Lee, M. Jszwik, A. Sabac, C. Gorecki "Study of internal stress
characteristics of optical quality silicon oxinitride thin films fabricated
by plasma-enhanced chemical vapour deposition", pp. 242-246, Mechatronics
2001, 5th Franco-Japanese Congress & 3rd European-Asian Congress, Besangon
(France), October 9-11, 2001

  b.. C. Gorecki, A. Sabac, M. Jszwik, S.S. Lee, "Characterisation of
internal stress of silicon oxinitride thin films fabricated by
plasma-enhanced chemical vapour deposition: applications in Integrated
Optics", Proc. SPIE Vol. 4596, pp 9-15, 2001.


  c.. M. Jszwik, C. Gorecki, A. Sabac, "Optical interferometry investigation
of internal stress and opto-mechanical characteristics of silicon oxynitride
thin films fabricated by PECVD", Symposium on Design, Test, Integration and
Packaging of MEMS/MOEMS, Cannes Mandelieu, France, 5-8 Maj, Proc. SPIE Vol.
4755, pp 760-764, 2002.
  Best regards

  Michal Jozwik




----- Original Message -----
From: "kakasaheb chandrakant mohite" 
To: 
Sent: Friday, June 28, 2002 8:16 AM
Subject: [mems-talk] Silicon oxynitride optical properties


> Dear friends,Dear MEMS colleagues
> I have deposited Silicon oxynitride thin films by
> EB-PVD.I would like to know the dependence of
> substrate temperature on compositional and optical
> properties (particularly refractive index and
> reflectance) of these films.
> Can someone point me to sources where optical
> properties of SiOxNy can  be checked?
>
> Thanks
> K.C.Mohite
>
> =====
> **********************************************************
> K.C.Mohite                          Ph.9120-5695201(O)
> School Of Energy Studies               9120-7291872(R)
> Department of Physics
> University of Pune
> PUNE-411 007
> INDIA
> Yahoo! - Official partner of 2002 FIFA World Cup
> http://fifaworldcup.yahoo.com
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
MEMS Technology Review
The Branford Group