A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Al evaporation
Al evaporation
2002-07-11
Zhihai Zhang
2002-07-12
Rick Williston
2002-07-12
Neal Ricks
2002-07-12
Milan Buncick
2002-07-12
[email protected]
Al evaporation
Neal Ricks
2002-07-12
 Zhihai,
I evaporate Aluminum right out of the hearth.
Neal
  Zhihai Zhang  wrote: Hello everyone,
I need do Al e-beam evaporation frequently.
However after several times, Al always spill out of the crucible and get the
crucible cracked. I use small ramp rate, it still happened.
How can I prevent it?
Thnaks,

Zhihai
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/
New! SBC Yahoo! Dial - 1st Month Free & unlimited access

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
Harrick Plasma, Inc.