I need to ectch gold away from the back of alumina template .Its about 1000A
thick, Please can any one suggest me the correct recipe.

fabbi.

PHANEENDRA MEDIDA
Research Assistant
Magnetic MEMS(Dr.Gary Friedman),
Drexel University,
Philadelphia PA 19104