adhesion of Ag to Si
Thomas B. Jones
2002-07-24
Dear MEMS community:

Is it true that Ag exhibits poor adhesion to Si, say for example, in
comparison to Al?  Will a thin layer of Cr help to improve this adhesion?
Finally, are there other straightforward methods to promote adhesion of
these materials?

Thanks.

Tom Jones


________________________________________________________
Thomas B. Jones
Professor of Electrical Engineering
University of Rochester
P.O. Box 270126
Rochester, NY  14627-0126    (USA)
phone: 1-585-275-5233   fax: 1-585-273-4919
email: [email protected]
http://www.ece.rochester.edu/~jones
________________________________________________________

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Nano-Master, Inc.
The Branford Group
Mentor Graphics Corporation