PECVD Si3N4 receipe
Roger Shile
2002-07-29
PECVD generally does not produce Si3N4, but rather a  witches brew of
silicon nitrogen and hydrogen ,often referred to as SixNyHz or just SiN.
For some reason I don't understand people usually adjust this composition to
get a refractive index of ~2, which is close to the index of Si3N4. SiN with
this index us usually very silicon rich.

A recipe I have used to synthisize SiN with n~2 in a Pacific Western Coyote
is as follows:

300 sccm silane (100%)
2000 sccm ammonia
Pressure = 2 torr (lower pressure improves uniformity, but raises stress)
R.F. power = 300 watts @25-450 kHz (This frequency range will result in a
film with compressive stress.  13.56 MHz excitation should result in films
with tensile stress)
Temperature = 380 degC)

Roger Shile

-----Original Message-----
From: Dlee Li [mailto:[email protected]]
Sent: Friday, July 26, 2002 1:36 PM
To: [email protected]
Subject: [mems-talk] PECVD Si3N4 receipe


Hi friend,
anyone can tell me one workable PECVD Si3N4 receipe? my system is
Plasma-Therm.

Thanks
Dlee
Mechanical Engineering Department
The University of Texas at Austin



_________________________________________________________________
Join the worlds largest e-mail service with MSN Hotmail.
http://www.hotmail.com
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/
"This email and any attachments may contain information that is confidential and
proprietary information of Veeco Instruments Inc. and are intended only for the
use of the addressee. Unauthorized use, distribution or copying is forbidden. If
you have received this email in error, please notify the sender immediately by
return email and delete all copies of this message and any attachments from your
computer. Thank you."

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Addison Engineering
Tanner EDA by Mentor Graphics
MEMS Technology Review