MEMSnet Home: MEMS-Talk: Convection coefficient
Convection coefficient
2002-08-09
Philippe HELIN
2002-08-22
Hengzi (David) Wang
2002-08-09
Michael D Martin
2002-08-22
Michael D Martin
Convection coefficient
Philippe HELIN
2002-08-09
Hi,

I am looking for value of convection coefficient between silicon and air for
thermal modeling, any idea ?
Thanks,
Philippe




_________________________________________________________________
Affichez, modifiez et partagez gratuitement vos photos en ligne:
http://photos.msn.com/support/worldwide.aspx

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
The Branford Group
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.