A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Adhesion of metal to epoxy substrates
Adhesion of metal to epoxy substrates
2002-08-07
Fred Hussain
2002-08-07
Greg Miller
2002-08-07
Bill Moffat
2002-08-09
Fred Hussain
2002-08-09
Bill Moffat
Adhesion of metal to epoxy substrates
Fred Hussain
2002-08-09
Bill,

It sounds like a good idea, but unfortunately the epoxy we use must not be
exposed to temperatures above ~60oC, otherwise it starts getting soft and we
lose our features. Can it be done at the lower temperature? What sort of
gases do you recommend, SF6 or CF4 as well as O2, Ar, N2? We use hexane to
remove silicone and have a plasma asher with the latter of the gases
connected, which is used just prior to the metallisation. Do you know of any
adhesion promoters (HMDS?) which would work on epoxy? Also, where abouts are
you based, USA?

Kind regards,

Fred.

-----Original Message-----
From: [email protected] [mailto:[email protected]]On
Behalf Of Bill Moffat
Sent: 07 August 2002 15:39
To: [email protected]
Subject: RE: [mems-talk] Adhesion of metal to epoxy substrates


Fred,
     This could explain a number of special units we have built with no
indication of the final use.  These are special Plasma/Silane deposition
units.  Think stainless oven set at 150 degrees C able to do vacuum priming
with flat capacitive stainless plasma generators for precleaning.  let me
know
if you want to test this approach.  Bill Moffat

-----Original Message-----
From: Fred Hussain [mailto:[email protected]]
Sent: Wednesday, August 07, 2002 1:31 AM
To: [email protected]
Subject: [mems-talk] Adhesion of metal to epoxy substrates


Dear Collegues,

I am looking for any advice/information on how to improve adhesion of
evaporated metal (nichrome + gold) onto thermo-epoxy based substrates. In
particular, information on chemical and physical (plasma) surface
pre-treatments and/or alternative metals which may have a distinct advantage
over nichrome and gold, would be highly appreciated.

Thanking you in advance,

Fred.
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
University Wafer
MEMS Technology Review