Has any body found a way to pattern relatively small features (3 m) on wafers
that already have deep trenches micromachined in them? We've experienced
problems with the photoresist "retreating" from the sharp edge of the trench,
causing a narrow window to open in the photoresist on the silicon at the edge
of the trench.

Perry Skeath
ITM, Inc.


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing