MEMSnet Home: MEMS-Talk: delamination of Au/Ni/Ge/Au layers in Citric acid solution etch
delamination of Au/Ni/Ge/Au layers in Citric acid solution etch
2002-09-05
Parshant Kumar
2002-09-06
Oray Orkun Cellek
2002-09-06
Tabada, Phillipe
delamination of Au/Ni/Ge/Au layers in Citric acid solution etch
Tabada, Phillipe
2002-09-06
Can you provide more specifics?  For example, what are the thicknesses of
the layers and what temperature was the anneal done and did the whole
electrode delaminate or everything except the bottom gold layer?

Phil Tabada

-----Original Message-----
From: Parshant Kumar [mailto:[email protected]]
Sent: Thursday, September 05, 2002 10:30 AM
To: [email protected]
Subject: [mems-talk] delamination of Au/Ni/Ge/Au layers in Citric acid
solution etch


Hi All,

I am working with the wet etch of GaAs in citric
acid:Hydrogen peroxide::5:1. I am facing the problem that
Electrode deposited as Au/Ni/Ge/Au layers start delaminated
after 55-60 mintues of etching. However if we anneal the
sample for 30 mintues at the 150 degree calcious, the
effect is less.

Any comment will be appericiated

Thx

Kumar
Maryland MEMS Lab
University of Maryland
College Park-MD 20742
Tel 301-405-0364


__________________________________________________
Do You Yahoo!?
Yahoo! Finance - Get real-time stock quotes
http://finance.yahoo.com

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/
DISCLAIMER: Unless expressly stated otherwise, this message is confidential and
may be privileged. It is intended for the addressee(s) only. Access, copying,
disclosure or re-use of the e-mail or any information contained therein by any
other person is not authorized. If you are not the intended recipient please
notify the sender immediately by returning the e-mail to the originator.


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
The Branford Group
MEMStaff Inc.