MEMSnet Home: MEMS-Talk: PDMS mixer/dispenser
PDMS mixer/dispenser
2002-09-06
Changsoon Kim
2002-09-10
Luke Hunter
PDMS mixer/dispenser
Luke Hunter
2002-09-10
We've made a little stirrer and attached it to a Dremel.  It does the
job quickly and thoroughly.

-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of Changsoon Kim
Sent: Friday, September 06, 2002 11:20 AM
To: [email protected]
Subject: [mems-talk] PDMS mixer/dispenser


Hi,

I would like to know where I can order a mixer/dispenser
to mix the prepolymer and the curing agent.

I have been using Sylgard 184 and have been mixing them manually with a
plastic rod.

Thanks,

Changsoon Kim
Princeton University.


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
University Wafer
Nano-Master, Inc.