2002-09-27
I have found hexane to be a satisfactory solvent for PDMS.


Good Luck

Danny

----- Original Message -----
From: "flavio" 
Date: Tue, 24 Sep 2002 00:23:25 -0500
To: 
Subject: [mems-talk] how to remove PDMS?


>
>
>             Hello everybody,
>
>             Does anybody know how to remove (strip, clean, dissolve,
> etc.)  PDMS other way than putting it in acetone? My problem is simple,
> I've PMMA with residues of PDMS that I want to get rid of. IPA didn't
> work.
>
>
>
>             Please send an email to [email protected]
>
>
>
>             Thanks,
>
>
>
> Flavio Aristone.
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>
>

--
__________________________________________________________
Sign-up for your own FREE Personalized E-mail at Mail.com
http://www.mail.com/?sr=signup



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
Nano-Master, Inc.