5" photomask making
2002-10-18
Jafar Haji Babaei
2002-10-22
Frank DiPiazza
2002-10-22
Kevin A. Shaw
2002-11-04
René Fléron
5" photomask making
Frank DiPiazza
2002-10-22
Jafar,
I have been using Photronics for years and have had great support from there
entire staff. Call:
Matt Traisci
[email protected]
203-740-5664 (office)
203-740-5601 (fax)

-----Original Message-----
From: Jafar Haji Babaei [mailto:[email protected]]
Sent: Friday, October 18, 2002 11:28 PM
To: [email protected]
Subject: [mems-talk] 5" photomask making




Can anybody suggest a reliable 5" photomask making company? I have lost my
contact with Lsiphotomask and looking to find a new reliable link.

Best Regards
Jafar



_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://www.memsnet.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
MEMS Technology Review