MEMSnet Home: MEMS-Talk: etching Si-N, but not Al2O3
etching Si-N, but not Al2O3
2002-10-22
Justin Borski
2002-10-22
[email protected]
2002-10-22
[email protected]
2002-10-22
Robert C Cole
etching Si-N, but not Al2O3
[email protected]
2002-10-22
> I wonder if somebody can suggest any etchants that
> etch PECVD Si-N, but do not etch or etch very slowly
> alumina coating. Thanks in advance for your help
> Honggang Jiang

We've looked at a number of wet etchants, but none of them will work.
An SF6-based plasma will work.
        --Kirt Williams Agilent Technologies


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Harrick Plasma, Inc.
The Branford Group
Process Variations in Microsystems Manufacturing