MEMSnet Home: MEMS-Talk: silicon/sio2/si3n4
silicon/sio2/si3n4
2002-10-28
Qintao Zhang
2002-10-29
Priyanka Aggarwal
2002-10-29
Atul Garg
2002-10-29
[email protected]
2002-10-30
[email protected]
silicon/sio2/si3n4
Priyanka Aggarwal
2002-10-29
Well according to me, it is difficult to deposit silcion nitride directly on
silicon , so it might be the reason for the same.

----- Original Message -----
From: "Qintao Zhang" 
To: 
Sent: Monday, October 28, 2002 6:14 PM
Subject: [mems-talk] silicon/sio2/si3n4


>
> Hi, all
>
> I am a new member on MEMS. I am trying to understand a capacitor structure
composed of silicon/silicon dioxide/ silicon nitride sandwich. I am
wondering why need a silicon dioxide layer in the middle? silicon nitride is
also a good insulator, why we need two insulators for a capacitance? Are
there big difference between silicon dioxide and silicon nitride, especially
on electrical property?
>
> Thanks a lot
>
> Qintao Zhang
>
>
>
> ---------------------------------
> Do you Yahoo!?
> Y! Web Hosting - Let the expert host your web
site_______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://www.memsnet.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
MEMS Technology Review