Clean-off Au/Sn solder from aluminum substrate
2002-11-04
Ken Yao
Clean-off Au/Sn solder from aluminum substrate
Ken Yao
2002-11-04
Dear All Members:

I am searching for a chemical or chemicals to clean-off or etch-off the
residual Au/Sn (78%/22% wt.) solder that stick in the pockets of aluminum
frame after vacuum / thermal  sealing (305°C). I want clean off the solder
only without any damage to the pockets (that is precisely machined).

Your input / comment / information are highly appreciated.

Kenneth S. Yao
Sr. Project Engineer
Statek Corp.
512 N. Main St.
Orange, CA 92868
(714) 288-3584


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
Addison Engineering