MEMSnet Home: MEMS-Talk: measuring thickness of thin organic layers
measuring thickness of thin organic layers
2002-11-05
Madanagopal K.V.
measuring thickness of thin organic layers
Madanagopal K.V.
2002-11-05
Hello,
Has anyone measured thin organic layers on gold (or other metals)?  I am
trying to measure ~40A thick films.  Would ellipsometry work?
I would appreciate if anyone could suggest some references.

Thanks
Madan

___________________________________________________________

K.V.Madanagopal, Ph.D.
Senior Research Associate
Alliance for Nanomedical Technologies
317 Stocking Hall
Cornell University
Ithaca
NY 14850
Fax:607-255-8741
Phone:607-254-8052
___________________________________________________________



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
MEMStaff Inc.