A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: special photolithography needed
special photolithography needed
2002-11-20
Enzhu Liang
2002-11-20
X. Yuan
2002-11-20
Christopher Blanford
2002-11-20
Greg Miller
2002-11-20
Bill Moffat
2002-11-20
BERAUER,FRANK (HP-Singapore,ex7)
2002-11-21
Alex Pozdin
special photolithography needed
Bill Moffat
2002-11-20
Enzhu,
      This could be difficult.  A possible but expensive answer may be a 3D
Holographic projection aligner.  Karl Suss used to manufacture one this gives
you the ability to use a variable focus and expose with the same intensity at
different focal lengths from the mask plane.  If you need more information I can
probably locate engineers who have used this sort of system for exposure down
the side of a steeply sloping line with the same C.D. at the top, down the
slope, and at the bottom of the slope.  Bill Moffat

-----Original Message-----
From: Enzhu Liang [mailto:[email protected]]
Sent: Tuesday, November 19, 2002 2:00 AM
To: [email protected]
Subject: [mems-talk] special photolithography needed


Hello everyone,

Can we do intentionally uneven exposure to the photoresist? Just imagine a
semisphere containing the photoresist and I am going to get uniform exposure on
the surface of the semisphere. This will require the UV light intensity stongest
in the center and weakest at the edges.If you happen to know this, could you
please tell me how to do it or suggest some reading about it? Thank you very
much.

Best regards,

        E.Liang





_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://www.memsnet.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Addison Engineering
Nano-Master, Inc.
Mentor Graphics Corporation