A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Through holes (vias) in quartz glass 4 " wafer?
Through holes (vias) in quartz glass 4 " wafer?
2002-11-28
Vincent Schneider
2002-12-02
BERAUER,FRANK (HP-Singapore,ex7)
2002-12-03
Wesselkamp, Carsten
2002-11-27
Anna-Sara Hedman
2002-11-27
sp
2002-11-28
Erik Jung
2002-11-27
[email protected]
2002-11-28
Vincent Schneider
Through holes (vias) in quartz glass 4 " wafer?
BERAUER,FRANK (HP-Singapore,ex7)
2002-12-02
Another low-cost quick and dirty method is sandblasting.
It can achieve down to 150um holes, but the edges are ragged
and not very accurate. It works well as ink-feed holes for our
Inkjets, but is not much used eleswhere.

Greetings,
        Frank Berauer
        Senior R&D Engineer
        Hewlett-Packard Singapore


-----Original Message-----
From: Michael D Martin [mailto:[email protected]]
Sent: Thursday, November 28, 2002 1:10 AM
To: [email protected]
Subject: Re: [mems-talk] Through holes (vias) in quartz glass 4 " wafer?


You have three options:
1) DRIE (Deep Reactive Ion Etching): This option will require a nice
thick resist. You can contact STS in the UK.
2) Laser Cutting: You can contact Lambda Physik in Germany.
3) Micromilling: We can micromill vias down to ~100 micron diameter.
But we're in Kentucky.

-Good luck
      Mike

>>> [email protected] 11/27/02 06:41AM >>>
Dear Sir/Madam,

Do you know how to make via holes - i.e. holes through
a quartz glass (fused silica) 4 " wafer, 525 microns thick?

Or do you know anybody else who can do this (in Europe if possible?)
by laser or ultrasonic drilling? Or any other technique?

I need to have approx. 160 holes in each wafer.
The wafer is covered with photoresist (or other masking material)
to mark the location of the through holes,  but also to protect
the bonding surface on the other side from mechanical scratch ...
The hole location is quite important...

I'll  be happy to hear from you soon !

Thanks!

Best regards








_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk

Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics