MEMSnet Home: MEMS-Talk: Laser Dicing
Laser Dicing
2002-12-03
Hugo Jazo
2002-12-04
Michael D Martin
2002-12-09
Randall Cha (Dr)
2002-12-10
Michael D Martin
Laser Dicing
Michael D Martin
2002-12-10
Hugo,
  You might try JPSA Laser at www.jpsalaser.com . Methods to avoid
surface contamination: laser machining in various reactive atmospheres
or simply leaving resist on the surface.

-Mike

>>> [email protected] 12/09/02 05:07AM >>>
Hi Hugo,

You may want to check out www.synova.ch.

They offer a water jet guided laser.

Rgds,
Randall

-----Original Message-----
From: Hugo Jazo [mailto:[email protected]]
Sent: Wednesday, December 04, 2002 12:02 AM
To: [email protected]
Subject: [mems-talk] Laser Dicing


Hello All,
Anyone know of a good laser dicing company out there?  Also, how do
people
deal with the debris that could contaminate sensitive mems devices on
the
surface?

-Hugo Jazo

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk

Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk

Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
MEMS Technology Review
University Wafer