Dear all,

I am looking for an etchant that etches silver but will not (or barely) etch
copper. I also would like an etchant for the reverse situation (Cu: yes, Ag:
no).

Best regards,
Gilbert Schuurman


Viasystems Mommers B.V.
Peutenweg 2
6101 VZ Echt
The Netherlands
tel. : +31 475 479-222
fax: +31 475 479-407
mailto:[email protected]
http://www.viasystems.nl




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
The Branford Group