electroless gold plating solution
Lester Lopez
2003-01-17
Kris,

Technic inc and Stapleton technologies have supplied us with electroless
nickel and gold plating solutions.  You might want to check them out at

www.technic.com

www.stapletontech.com


Lester López
Research Assistant
Microwave and Wireless Research Center
University of South Florida
4202 East Fowler Avenue, ENB 118
Tampa, Florida 33620
PH: 813-974-4851
FAX: 813-974-5250
Email: [email protected]
----- Original Message -----
From: "krishna arvindan" 
To: 
Sent: Thursday, January 16, 2003 3:13 PM
Subject: [mems-talk] electroless gold plating solution


>
> Hi,
>
> Can someone suggest me regarding vendors who can supply electroless gold
plating solution.
>
>
>
> Thanks
>
> kris
>
>
>
>
>
> ---------------------------------
> Do you Yahoo!?
> Yahoo! Mail Plus - Powerful. Affordable. Sign up now
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Addison Engineering