MEMSnet Home: MEMS-Talk: indium alloys - deposition and patterning
indium alloys - deposition and patterning
2003-02-21
[email protected]
2003-02-24
Shay Kaplan
2003-02-24
Bill Moffat (4 parts)
indium alloys - deposition and patterning
Shay Kaplan
2003-02-24
If the indium geometries are not too small, you can evaporate them through a
shadow mask.
shay

[email protected] wrote:

> Indium can easily be evaporated to those thicknesses. We have built
evaporators for this purpose. I don't know how to etch the material but you
could use a lift-off technique with thick photoresist. Maybe Bill Moffet can
provide some insights to lift-off with those thicknesses. Bob Henderson
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
MEMS Technology Review