MEMSnet Home: MEMS-Talk: seeking services: dep of thick insulators
seeking services: dep of thick insulators
2003-03-07
John Chiaverini
seeking services: dep of thick insulators
John Chiaverini
2003-03-07
I'm seeking a company or fab that can handle small batches and can deposit
10-20 um of any of the following  materials onto an insulating substrate:

sapphire
glass/SiO2
quartz
alumina
aluminum nitride
diamond

or other low rf-loss material that can be etched.

Thanks, you can contact me directly.


John Chiaverini
NIST Boulder, Time and Frequency Division
Ion Storage Group, Quantum Computation Project
[email protected]
(303) 497-4364


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Tanner EDA by Mentor Graphics
MEMS Technology Review
Harrick Plasma, Inc.