MEMSnet Home: MEMS-Talk: Re: looking for SOI wafers
Re: looking for SOI wafers
2003-04-07
lucia beccai
2003-04-08
Andrew Kuchling
2003-04-08
Sunil Kumar
2003-04-08
Lawlor, Chris
2003-04-08
Renie Duvall
2003-04-09
[email protected]
Re: looking for SOI wafers
Lawlor, Chris
2003-04-08
Analog Devices Belfast also carry an inventory of SOI stock- we would be
happy to supply a list detailing current availability.

Best wishes,
Chris.



-----Original Message-----
From: lucia beccai [mailto:[email protected]]
Sent: 07 April 2003 13:17
To: Jing Liu
Cc: [email protected]
Subject: [mems-talk] Re: looking for SOI wafers


Hi Jing,
you can look up at:
http://www.universitywafer.com
they usually have all types of wafers at good prices.

Regards,
Lucia Beccai

--
----------------------------------------------
Lucia Beccai, PhD
CRIM Lab
Polo Sant'Anna Valdera
Scuola Superiore Sant'Anna
Viale Rinaldo Piaggio 34 - 56025 -Pontedera (Pisa) - Italy
phone: +39 050 883 488
fax  +39 050 883 402
http://www-crim.sssup.it/



_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/





reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
Addison Engineering
Tanner EDA by Mentor Graphics