Hello,
Is there any common release material that would help in release an
electroformed stamp from a plastic (polystyrene, polycarbonate) substrate
after stamping?  I find that some material remains after a stamping run.

thanks
Madan.

___________________________________________________________

K.V.Madanagopal, Ph.D.
Senior Research Associate
Alliance for Nanomedical Technologies
311 Stocking Hall
Cornell University
Ithaca
NY 14850
Fax:607-255-8741
Phone:607-254-8052
___________________________________________________________


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
MEMStaff Inc.
MEMS Technology Review
The Branford Group