MEMSnet Home: MEMS-Talk: SV: [mems-talk] Quartz glass and HRSS wafer requested
SV: [mems-talk] Quartz glass and HRSS wafer requested
2003-04-12
[email protected]
SV: [mems-talk] Quartz glass and HRSS wafer requested
[email protected]
2003-04-12
For the high resistivity silicon wafers you can contact Topsil in
Frederikssund. We manufacture silicon by the Float zone method up to 15.000
Ohmcm, and we might have some extra wafers on stock. Try our sales
department at [email protected].

Best regards,

Jan Vedde

Topsil Semiconductor Materials A/S
Linderupvej 4 * P.O. Box 100
DK-3600 Frederikssund * Denmark
Phone: +45 4736 5600 (switchboard)
Telefax: +45 4736 5601


-----Oprindelig meddelelse-----
Fra: Oberhammer Joachim [mailto:[email protected]]
Sendt: 11. april 2003 10:30
Til: [email protected]
Emne: [mems-talk] Quartz glass and HRSS wafer requested

Hi people,

I'm looking for quartz glass (and no other type of glass) and for
high resistivity silicon substrates (>=3000 Ohm cm), both 100 mm
(probably also smaller), thickness about 500 um.
Volume: 3-5 pieces.
Does anybody know companies delivering low quantities of these
substrates? Does anybody of you have some of them in your stock and
you'd like to get rid of them?

Thanks for your help,
--
----------------------------------------------------------------------------
--
Joachim Oberhammer, Dipl.-Ing.

Royal Institute of Technology (KTH)   Phone:    +46/(0)8 790 6250
Dept. of Signals, Sensors and Systems Fax:      +46/(0)8 10 0858
Microsystem Technology (MST)          Mobile:   +46/(0)70 692 1858
                                       e-mail:
[email protected]
Osquldas väg 10                       homepage: http://www.s3.kth.se/mst/
SE-100 44 Stockholm, Sweden

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics