MEMSnet Home: MEMS-Talk: dialectric coatings
dialectric coatings
2003-04-11
[email protected]
2003-04-14
Likun Zhu
2003-04-15
Shay Kaplan
dialectric coatings
Likun Zhu
2003-04-14
Try polyimide. There are photosensitive or
unphotosensitive polyimide.
--- [email protected] wrote:
> Hi.
> I am looking for a dialectric coating to deposit on
> a gold pad array.  I
> thought about parylene, but it is not cost
> effective.  Is there possibly
> some spin on glass or something of the sort that
> does not have to bake at
> 400+?
> Thank you,
> Kelly
>
> --
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe
> or change your list
> options, visit
>
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS
> processing services.
> Visit us at http://www.memsnet.org/


__________________________________________________
Do you Yahoo!?
Yahoo! Tax Center - File online, calculators, forms, and more
http://tax.yahoo.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Mentor Graphics Corporation