Dear all,

I am looking for a company in Europe that provides fusion bonding for 4
inch Silicon wafers.
Thank you
Vittorio

***************************
Ing. Vittorio Guarnieri
ITC-Irst
MIS MIcroSystem division
Via Sommarive, 18
38050 Povo (Trento)
Italy
Tel.    0039 0461 314468
Fax.    0039 0461 314539
Mobile. 0039  338 9267510
e-mail [email protected]
***************************


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
The Branford Group
Process Variations in Microsystems Manufacturing