View Mailing Online
MEMS technology
- With new design, bulk semiconductor proves it can take the heat: Thin-film ...
- The intense interest in harvesting energy from heat sources has led to a renewed push to discover materials that can more efficiently convert heat into electricity. Some researchers are finding those gains by re-designing materials scientists have been ...
yesterday Nanotechnology News (press release) - MEMS technology
- Thin-film process boosts bulk alloy's thermoelectric performance
- The alloy in question, Silicon Germanium, has been valued for its performance in high-temperature thermoelectric applications, including its use in radioisotope thermoelectric generators on NASA flight missions. But broader applications have been ...
yesterday Next Big Future - MEMS technology
- Joint Project to Develop Innovative Process for Producing Large-Area Polymer Films
- By Cameron Chai A joint project, PolAR has been initiated by the Fraunhofer FEP and the Fraunhofer IOF along with their industrial partners, including Southwall Europe, Rodenstock and Leica Microsystems, to develop an innovative, ...
today Azom.com - MEMS technology
MEMS business
- Carnegie Mellon University Plays Host to MEMS Industry Group with Microsystems ...
- ... WIRE) -- MEMS Industry Group (MIG) is bringing the global micro-electromechanical systems (MEMS) supply chain to Pittsburgh for its annual meeting, giving leading MEMS suppliers an opportunity to tour Carnegie Mellon's microsystems labs on May 8.
yesterday MarketWatch (press release) - MEMS business
- SEMATECH Technologists Demonstrate Breakthrough Process Solutions for ...
- SEMATECH experts reported on innovative approaches to realize advanced CMOS logic and memory device technologies and 3D through-silicon via (TSV) manufacturing at the International VLSI Technology, System and Applications Symposium (VLSI-TSA) on April ...
yesterday Virtual-Strategy Magazine - MEMS business
- GLOBALFOUNDRIES Fab 8 Adds Tools to Enable 3D Chip Stacking at 20nm and Beyond
- The TSV capabilities will allow customers to stack multiple chips on top of each other, providing another avenue for delivering the demanding requirements of tomorrow's electronic devices. Essentially vertical holes etched in silicon and filled with ...
today MarketWatch (press release) - MEMS business
- Advanced memory and logic tech and 3D TSV by SEMATECH at VLSI Sympo
- Sitaram Arkalgud, director of SEMATECH's 3D Interconnect program revealed copper-to-copper direct bonding (CuDB) technology as a technology to scale chip-to-chip interconnects and keep pace with advances in TSV. 1. Evaluating stress-induced leakage ...
today EE Herald - MEMS business
- Medical 'Lightsabers' to Be Presented at CLEO: 2012
- The optics consist of three parts: commercial lenses; a specialized fiber to deliver the ultrashort laser pulses from the laser to the microscope; and a 750-micrometer MEMS (micro-electro-mechanical system) scanning mirror.
today OptoIQ - MEMS business
- Magnetic MEMS under development at Silex thanks to new research grant
- April 25, 2012 - PRNewswire -- Silex Microsystems, a pure-play micro electro mechanical system (MEMS) foundry, will develop ferromagnetic materials for next-generation MEMS devices, under a new VINNOVA research grant worth nearly 3 million Swedish ...
yesterday ElectroIQ - MEMS business
- Research and Markets: Global Automotive MEMS Market 2011-2015 ...
- DUBLIN--(BUSINESS WIRE)--Dublin - Research and Markets (http://www.researchandmarkets.com/research/bchvp8/global_automotive) has announced the addition of the.
Business Wire today - MEMS business
- Carnegie Mellon University Plays Host to MEMS Industry Group with ...
- Carnegie Mellon University Plays Host to MEMS Industry Group with Microsystems' Lab Tours. ... Carnegie Mellon University Plays Host to MEMS Industry Group with Microsystems' Lab Tours - on ...
yesterday - MEMS business
Nanotechnology
- Nanotech is Making Water Testing Quicker & Easier
- This science of manipulating fluids at the micro-scale, called microfluidics, has been widely applied to chemical separations, most notably to analyze genes. In OndaVia's novel approach, the etched channel is not of a uniform width; its width varies, ...
yesterday LiveScience.com - Nanotechnology
- New nanomaterial-based magnetoelectric sensors for deep brain ...
- Posted: Apr 26th, 2012. New nanomaterial-based magnetoelectric sensors for deep brain stimulation. (Nanowerk News) Up to now, the brain's magnetic field is measurable only under technical laboratory conditions. This technique is therefore ...
today - Nanotechnology
- Researchers Exploit Graphene's Electrical Conductivity to Develop High ...
- Graphene is a two-dimensional nanomaterial with superior properties. Yun Hang Hu, one of the researchers, informed that graphene's high electrical conductivity makes it a crucial element to develop future generation solar panels.
today Azom.com - Nanotechnology
Featured Event
September 12-13, 2012. Meet with the best, the brightest, the innovative; they are the hard-to-reach industry thought-leaders.
At MEMS in Motion, you won't have to hope you'll make the right connections -- you'll know long before you arrive!
Event Calendar
- M2M Forum Webinar: Market Pull vs. Technology Push
- 2012-04-27
Online 11:30 AM ET, 8:30 AM PT LOWER cost and SHORTER time without reinventing the wheel
|
|
- M2M Forum 2012 (MEMS Industry Group)
- 2012-05-08 - 2012-05-09
Pittsburgh PA Focus on Technical Challenges to MEMS Commercialization
|
|
- MEPTEC MEMS Technology Symposium 2012
- 2012-05-23
San Jose CA
|
|
- MEMS Business Forum 2012
- 2012-05-24
Santa Clara CA The premier MEMS business development and networking event
|
|
- Design Automation Conference (DAC) 2012
- 2012-06-03 - 2012-06-07
San Francisco CA
|
|
- Hilton Head Workshop 2012
- 2012-06-03 - 2012-06-07
Hilton Head Island, SC A Solid-State Sensors, Actuators and Microsystems Workshop Visit MNX at this event.
|
|
- Sensors Expo & Conference 2012
- 2012-06-06 - 2012-06-07
Rosemont (Chicago) IL Providing over 25 Years of Technical Innovation & Thought Leadership
|
|
- IMS 2012 International Microwave Symposium
- 2012-06-17 - 2012-06-22
Montreal Canada Celebrate the 60th anniversary of both the Microwave Theory and Techniques Society and the International Microwave Symposium
|
|
- ACTUATOR 2012
- 2012-06-18 - 2012-06-20
Bremen, Germany International Conference and Exhibition on New Actuators and Drive Systems
|
|
- TechConnect World Summit & Innovation Showcase
- 2012-06-18 - 2012-06-21
Santa Clara CA Increase your Innovation Pipeline!
|
|
- SEMICON West 2012
- 2012-07-10 - 2012-07-12
San Francisco CA Connect to Buyers, Grow your Business!
|
|
- 45th Int'l Symposium on Microelectronics
- 2012-09-09 - 2012-09-13
San Diego CA Bringing Together The Entire Microelectronics Supply Chain!
|
|
- MEMS in Motion Collaboration Summit
- 2012-09-12 - 2012-09-13
Palm Springs, CA Collaboration & Networking on Steroids!
|
|
- SENSORS Tech Forum '12
- 2012-10-01 - 2012-10-03
Anaheim, CA The Sensors Technology Industry Is Abuzz... Find Out What All the Buzz is About
|
|
- AVS 59th International Symposium and Exhibition
- 2012-10-28 - 2012-11-02
Tampa Florida
|
|
- MEMS Executive Congress US 2012
- 2012-11-07 - 2012-11-08
Scottsdale AZ
|
|
- PowerMEMS 2012
- 2012-12-02 - 2012-12-05
Atlanta, Georgia The 12th International Workshop on Micro and Nanotechnology for Power Generation and Energy Conversion Applications
|
|
- SPIE Photonics West 2013
- 2013-02-02 - 2013-02-07
San Francisco CA The Conference and Marketplace for the Photonics, Biophotonics, and Laser Industry
|
|
- SPIE Advanced Lithography 2013
- 2013-02-24 - 2013-02-28
San Jose, CA The world's premier semiconductor lithography conference and exhibition
|
|
|
|