MEMSnet Home: MEMS-Talk: Alumina Etchants
Alumina Etchants
2003-05-06
Louis Chomas
2003-05-07
Absara Micro Systems
2003-05-06
Rodger Cary
Alumina Etchants
Rodger Cary
2003-05-06
There is a book called "Alumina As A Ceramic Material" put out by The
American Ceramic Society.  It has some good general information on Alumina
and Alumina coatings.


----- Original Message -----
From: "Louis Chomas" 
To: 
Sent: Tuesday, May 06, 2003 12:05 PM
Subject: [mems-talk] Alumina Etchants


>     I'm trying to etch some alumina films and was wondering if anyone
> had any suggestions for etchants or thoughts on where I could look to
> get some information/data on etching alumina.
>
> Thanks,
> Lou Chomas
>
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
Nano-Master, Inc.
Mentor Graphics Corporation