Alumina/ss
2003-05-22
:(): oxxxxxx|
2003-05-27
Absara Micro Systems
2003-05-25
Phillipe Tabada
2003-05-27
Absara Micro Systems
Alumina/ss
Absara Micro Systems
2003-05-27
Use organ gas plasma etch after resist patterning. Alumina can be etched
using organ gas plasma.
Gautham at [email protected]

----- Original Message -----
From: ":(): oxxxxxx|" 
To: 
Sent: Thursday, May 22, 2003 11:49 PM
Subject: [mems-talk] Alumina/ss


>   hi.
>
>   I depositing a alumina thin film on the surface of Stainless Steel. I
tried to have a look of the cross section. Anybody can tell me how to etch
it?
> --
> _______________________________________________
> Sign-up for your own FREE Personalized E-mail at Mail.com
> http://www.mail.com/?sr=signup
>
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
MEMS Technology Review
The Branford Group