bonding
2003-06-18
mems greenhorn
2003-06-25
Yun Xi
bonding
mems greenhorn
2003-06-18
I have a microchannel etched on a quartz substrate ..the chip size is 1cm x 3cm
with gold layer on it which was a masking layer during the glass etch.For the
capping wafer I am using a microscope glass slide. At present I use epoxy at the
edges to bond the glass slide to  the chip.There is no leakage out of the
channel this way.But at the interface i.e at area of contact between the surface
of the chip and the top slide some liquid seeps in.Is there any simple solution
to prevent this ?


---------------------------------
Do you Yahoo!?
SBC Yahoo! DSL - Now only $29.95 per month!
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
MEMStaff Inc.
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing