Hi Sunny,

MemGen's EFAB technology has similarities to stereolithographic techniques.

http://www.memgen.com

Best Regards,

Art
__________________________________________________________________
Arthur S. Morris III, Ph.D.              [email protected]
CTO, VP Eng.                             v: 1-919-657-8101
wiSpry, Inc.                             f: 1-919-854-7501
4001 Weston Parkway, Suite 200           http://www.wispry.com/
Cary, NC 27513


> -----Original Message-----
> From: [email protected]
> [mailto:[email protected]]On Behalf Of
> [email protected]
> Sent: Friday, June 20, 2003 7:40 PM
>
> ----------------------------------------------------------------------
>
> Message: 1
> Date: Thu, 12 Jun 2003 10:39:01 -0400
> From: "il-seok Son" 
> Subject: [mems-talk] Streolithography.
> To: 
> Message-ID: 
> Content-Type: text/plain;     charset="iso-8859-1"
>
> Dear members,
>
> Would you recommend any foundry service capable of making small parts with
> stereolithography (SLA) in US.
> "Small" means MEMS scale.
>
> Thanks.
> __________________________________________________________
> Il-seok  Son (Sunny)
> Dept. of Electrical and Computer Engineering
> University of Wisconsin - Madison
> Office)  Sonic MEMS Lab,
> __________________________________________________________
>
>
> ------------------------------
>
>
> End of MEMS-talk Digest, Vol 8, Issue 13
> ****************************************


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Addison Engineering
MEMStaff Inc.
Process Variations in Microsystems Manufacturing