MEMSnet Home: MEMS-Talk: about BOE
about BOE
2003-06-25
Yun Xi (2 parts)
about BOE
Yun Xi
2003-06-25
Please check attachment. I had same experimence with soda lime. It is not
bad. Hard-baking is important. Try!

Xi


-----Original Message-----
From: Zhang
To: General MEMS discussion
Sent: 5/20/2003 2:43 AM
Subject: [mems-talk] about BOE

hi:

Who know how to use BOE etch 3000A glass.
thank you

Zhang
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

fab-micro-on s-l glass.pdf (application/octet-stream, 741376 bytes)
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
Addison Engineering
Tanner EDA by Mentor Graphics