MEMSnet Home: MEMS-Talk: PR strip after Mo etching
PR strip after Mo etching
2003-07-05
Koo Myung Kwon
2003-07-07
[email protected]
PR strip after Mo etching
[email protected]
2003-07-07
You can try removal in the same asher using forming gas. Try either a premix
with 94% Nitrogen+ 4% Hydrogen. If that is not feasible for you then try removal
with Argon in an rie mode. Might take longer but it should work. Bob Henderson