selective etching on ITO and Au
2003-09-26
Xiaoshan Zhu
2003-09-29
Customer Service
selective etching on ITO and Au
Customer Service
2003-09-29
Transene Company manufactures ITO Etchant TE-100 which will selectively
remove ITO from Au.  Please visit our website www.transene.com or contact me
for more information.

Sincerely,

Christopher Christuk
Transene Company
Tel:  978 777 7860
email:  [email protected]
----- Original Message -----
From: "Xiaoshan Zhu" 
To: 
Sent: Friday, September 26, 2003 1:56 PM
Subject: [mems-talk] selective etching on ITO and Au


> Does anyone have good recipe or good idea to selectively etch ITO and Au
on
> glass wafer? I'd keep Au but remove ITO.
>
> Thanks in advance!
>
> Xiaoshan
>
>
>



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Addison Engineering
Tanner EDA by Mentor Graphics